PU - POLYURETHANE - PHYSICAL PROPERTIES
  ETL91A / Moca
Hardness (Shore A) 90 +- 3
Tensile Strength (MPa) 25.5
    100% Modules (MPa) 6.2
    200% Modules (MPa) --
    300% Modules (MPa) 11.7
Angle Tear Strength (DIE C) (kN/m) 80
Trouser Tear Strength (DIE C) (kN/m) --
Elongation (%) 390
Resilience (DIN) (%)  
Abrasion (DIN) mm3  
Cured Density (g/cm3) 1.10
Compression set (22 hours @ 70C0) (%) 45